  1. What temp are you curing at? Tin melts at 450,I cure at 350 for 20 min.
  2. I use the same vibrator it works excellent, I use two heavy duty elastics so I can move it to different fluid beds.
  3. I would make the shaft a wee bit longer at least 1/4 to 3/8 longer
  4. Luremaking.com carries them.
  5. You should try craft paint.I use one called Craftsmart premium satin acrylic paint got it at Michaels, it will take heat to 350 degrees, powder paint jig heads as usual then apply the eye with nail let dry then apply the pupil (different color) then put jigs in oven to bake I do mine 360 degrees for 20 min.The acrylic paint melts into the head and can't scratch off.
  6. I use a craft paint called craftsmart (michaels sells it)after powder painting my jigs I use craftsmart to put the 2 color eyes on.You can put it in the toaster oven 350 degrees for 20 min,it doesn't run and seems to melt into the powder paint you cant scratch it off.
  7. Luremaking.com in ontario carries them.
  8. On a blown up picture of the jigs looks like a regular jig hook,but it looks like the hair is in the lead you cant see any thread.
  9. They also carry nail foil.
  10. Have you looked at Ali express "holographic heat foil"?
  11. Is there any place to buy bulk spools of 210 danville?
  12. When I clean out my pot, I take a drill bit same size as pour spout and ream it out there is a lot of rust that comes out,my pot hardly drips after.
  13. Google roto metals for prices. Also lead melts at 621 deg and bismuth at 520 deg.
  14. I wonder if it's salt water that causes it or is it dragging in the sand every once in a while causing it.I don't fish salt water,and my jigs looses its shine when bouncing off a sandy bottom when fishing walleye.
  15. I use the black but thin it with clear gloss,comes out really shinny.I aso have a vibrator on my fluid bed with the air.
  16. I dye a lot of the leftover brown buctails to black.
  17. Luremaking.com has them listed,but they are a Canadian co.
  18. cs coatings (component systems) has a fluid bed that will do up to 130 jigs (depending on size) at once.
  19. By the time you add the exchange rate its about the same price.
  20. Try Luremaking,com they are north west of Toronto.
  21. You did notice the original post is 10 yrs old.
×
×
  • Create New...
Top