I seal mine with D2T, then airbrush with Createx (water based).

#22 pizza

pizza

    Member

  • TU Member
  • PipPip
  • 197 posts

Posted 08 February 2012 - 05:38 PM

Paint the foil then seal.

Or seal(coat), then paint, then seal again (i prefer this method since the paint appears smoother).

#23 Mordy

Mordy

    New Member

  • TU Member
  • Pip
  • 9 posts
  • Location:
    Australia

Posted 09 February 2012 - 02:45 AM

Thanks for that, will try.
Lots of "product" flying around the site Etrex ??? (a GPS systen down here :)) and D2T sounds like a defoliant used in the vietnam war or something used for spraying Blackberries
All good, I have been sealing with a rod binding epoxy working well so far.
Thanks again

Edited by Mordy, 09 February 2012 - 02:46 AM.


#24 crankpaint

crankpaint

    Member

  • TU Member
  • PipPip
  • 248 posts
  • Location:
    w.v

Posted 10 February 2012 - 01:53 AM

e-tex is the short name for the epoxy used to pour on table tops to get a thick finish on them