I have recently been having problems with some of my molds producing a consistent laminate ie. craws. worms, brush hogs- But my top port injection swim baits ( basstackle 4&5" splittbellys and 631) are prodcuing as good as they ever had, Naturally my temperatures are consistent with this system, usually run around the 300 mark but have tried everything from 260-360 to try and find a solution but to no avail. I have tried to raise and lower the temperatue of one pot compared to the other-no change. I did not experince the aforementioned inconsistencies when I was using a blending block nor do I currently experience them with top injection molds. Any assistance in this matter would be greatly appreciated, I sell in multiple retail settings and I cannot market the current product that we are making. Thank you and have a great day.