    Mold Material?

    The rhordorsil can be gotten rfrom bluestarsilicones. I am going to try aeromarine products, they list a pourable high temp silicone am160 which they say is good for lead temps. Ted
  2. tedg

    Mold Material?

    David, I tried to find Rhodasill V330 on internet search, comes up blank, any more info? Thank you Ted
  3. Yes I buy theirs. They have white, flat black, red and yellow @ about $4.99 lb. I use that to undercoat as well as top coat on some. The web site I was thinking about had several colors ranging from $8 on sale to $18 regular. Thank you Ted
  4. I only make ocean fishing tackle. I use a lot of powder paint to paint my jigs. a few months ago, someone listed a site that sold larger quantities of powder. I remember checking out the site and I thought I had saved to my favorites. I also remember they were running specials for 1 lb. containers for several different colors. I don't believe they specialized in paints for tackle. Any info would be appreciated. Thank you Ted
  5. I have only fished saltwater. Mostly make jigs for my own use. Been casting 5 to 16 oz bullet jigs. I have been using LC molds to make the 8" twintail, but would like to find mold to make something similar to Kalin's big n grub, a 10" grub or something to Berkley's 8" powerbait saltwater grub. Wan to do some halibut fishing this summer. Thanks in advance. Ted
  6. You posted you wanted to get your tubes thicker. If that is what you meant, then just dip them more. Every dip adds to the thickness. I don't believe thickness has anything to do with hardness. Ted
×
×